For GTAW process i have PQR for P no1 Gr. no.1 joining to other metal P no.1 Gr. no.1

For our project Impact Testing is not specified in this condition is following interpretation is correct?

Is the above PQR will also qualify the following

1) P no. 1 Gr. no 1  with P no.1 to Gr. no. 2

2) P no. 1 Gr. no 2 with P no 1 Gr. no.2

3) P no 1 Gr. no.1 with P no 1 Gr. no.1

Kindly help me on above interpretation

Tush



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...