Set-through Nozzle Installation (application to pressure equipment):
WPS:
Must be qualified to weld thickness T .
There is no consideration of D , d or t .
Welder/Machine Welding Operator:
Must be qualified to weld in the position required and the
groove thickness T .
There is no consideration of D , d or t .
2. Set-on Nozzle Installation (application to pressure equipment):
WPS:
Must be qualified to weld thickness t .
There is no consideration of D , d or T .
Welder/Machine Welding Operator:
Must be qualified to weld thickness t .
Must be qualified to weld diameter d .
Position of welding must also be considered.
On Mon, Feb 24, 2014 at 10:08 AM, Rana Vikas <vhrana@gmail.com> wrote:
--Dear All,We have WPS 6'' NB X10.97 mm Sch 80 A106 Gr.B to 6'' NB X10.97 mm Sch 80 A106 Gr.B with GTAW + FCAW.
Can we use this WPS for branch joints i.e main Header (6'' NB X10.97 mm Sch 80 A106 Gr.B) to Pipe joints (3'' NB X 5.49 mm SCh.40 A106 Gr.B) ?
With Regards,
Vikas Rana
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments