Please find below the simple steps for oncoming material inspection.

a)      What are all the points to be inspected and verified during incoming inspection?

1)      Material required certificate or not, If yes receive certificate

2)      If material comes without certificate…Hold until receive

3)      Visual Inspection for damage

4)      Review certificate with applicable code and original marking

5)      Check dimension

6)      Check for any NDE requirement as per code or project specifications

7)      Prepare Incoming inspection reports

8)      Review reports

9)      Prepare inspection notice (if witness needed by the customer or AI/Third party)

10)   If the above points are accepted, release for fabrication

 

For acceptance criteria see applicable code of construction.For example,If ASME is construction code - refer to Sec.-II part A and the construction code.

 

Thanks & Regards,

 

(Karthik)



 
Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 9/29/10, muthu barathi <muthu_barathi@rediffmail.com> wrote:

From: muthu barathi <muthu_barathi@rediffmail.com>
Subject: Re: Re: [MW:7263] raw material
To: materials-welding@googlegroups.com
Date: Wednesday, September 29, 2010, 10:58 AM


Hi,

While verification first see whether you have recd materials according
to your PO conditions along with you material spec. then verify MTC,
then according to your material type grade , SA 6, SA 20verify .

According to your project spec carry out other check test as applicable
code.

Muthu Barathi P
Senior Manager QA/QC
AFCONS
On Wed, 29 Sep 2010 09:13:21 +0530 wrote
>Hi,
If the construction code is ASME,Then refer with ASME Sec.-II Part-A
for the applicable raw material and the applicable construction code.

Thanks & Regards,

(Karthik)
>
>
Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282
>
>--- On Tue, 9/28/10, Bhuvan Easwari wrote:
>

>From: Bhuvan Easwari
>Subject: [MW:7255] raw material
>To: materials-welding@googlegroups.com
>Date: Tuesday, September 28, 2010, 9:18 PM
>
>
Dear sir,
>During raw material verification what are the points to be inspected
and if you noticed any surface irregularities which code you have to
refer for acceptance/ not acceptance? Please clear my doubts.
>Thanks and regards
>VK.Bhuvan
>
--
>To post to this group, send email to materials-
welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

P Muthu Barathi
Mobile No:09967300544
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...