[MW:7289] RE: 7267 difference between E7018 and E7018-1

Dear Adi,

The designation of 1 in E 7018-1 represents that the electrode will meet the Charpy V-Notch Impact toughness
requirements at low tempearture. Actually, 7018-1 has better toughness at very lower sub-zero temperature as
well as more Manganese content than E7018.  

The purpose of having higher Mn% is to reduce the Ductile/Brittle Transition Temperature and to improve the low
temperature impact values of the weld metal.

The E 7018 will offer impact value of 47 Joules at -30 degree celcius and E7018-1 will give 47 joules at -50 degree
celcius.

Thanks and Regards,

Mani SarojKumar.
    

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...