Tuesday, September 28, 2010

[MW:7253] RE: 7230] Consumables to Base Metal

Larry,

 

ASME Section IX is a qualification document and not a design guide.  Once you have chosen your electrode/consumable and base metal(s), you qualify a WPS in accordance with the rules  of Sc IX and any other overriding design Code rules.  The consumable is limited to the A# and F# of the consumable used for the qualification testing.   If the consumable is an “unlisted” (i.e. not specified in Section Part C) one then it is limited to brand and type or specific chemistry.

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Larry
Sent: Monday, September 27, 2010 6:57 PM
To: materials-welding@googlegroups.com
Subject: [MW:7230] Consumables to Base Metal

 

Hi there,

 

Can anybody pointed me out to which clause in ASME IX that says that a certain consumables (Electrode) would be able to weld a certain base metal.

 

Your response is very much appreciated.

 

 

Thanks,

 

Larry

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...