Re: [MW:7203] use of E 7018 Electrode for stuructural welding without proper drying and holding

For Drying is only for control of Hydrogen induced crack in the weld metal , For that only Low hydrogen electrodes are to be Baked & Dried. It will not affect the Chem & Mech properties.
 

175, R.Kesavamoorthi,

Principal surveyor,

Quest (pvt.) Ltd.,

Ranipet.




From: asad azmi <azmiasadayub@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, 26 September, 2010 9:38:22 AM
Subject: [MW:7196] use of E 7018 Electrode for stuructural welding without proper drying and holding

Dear All,
 
Goodday.
 
 
what will be the effect in Mechanical/chemical proerties of deposited weld metal of  E7018 which is used for Structural welding of angle bar( material CS) without drying  (at 260-430deg C) and Holinding(at 120 deg C).
 
 
Can E7018 be used without proper drying and holding for stuructural welding( fillet weld only) of angle bar/supports(material CS).
 
 
Thanks in advance for your valuable suggestions.
 
Best  Regards
 
Asad Azmi
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...