Wednesday, September 29, 2010

[MW:7260] problem SS 316 flange to pipe welding

thank you mr porohit 
sending here with the drg of the same 
preparation done are 

rough m/c of the flange face & od 
step inside the flange to suit the length of the job the id of the step maintained was such that the pipe was press /tight fit in side the flange 
welded by gtaw as per details given in earlier mail



--
Regards
S.B. Badami
RMS Engineering
11/1 Shanti Nagar Bhosari
cell no +919850920429
+912027127939
visit us at www.indiamart.com/rmsengineering/

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...