Dear Praveen,

You can always use WNRF Flange of same Size & Pressure rating in place
of SORF. As WnRF is superior Joint ,it is used for High pressure
Service & when RT is required .
Plz take prior deviation from your Client.

Regards,


Vineet Kumar

On Tue, Sep 28, 2010 at 10:16 AM, Praveen Kumar
<praveenkumar.sek@gmail.com> wrote:
>
>
> Dear all,
>
>
>
> As per Material Specification (PMS) provided the materials 4"#150 SORF &
> IS-1239 pipe but  In this material shortage it is possible to be placed 4"
> WNRF flange same class for Fire water service pie line, Which is acceptable
> as per standards. Pls. guide me in this issue.
>
>
>
>
>
> Regards,
>
>
>
> Praveen Kumar
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...