Hi,

No body can say productivity norms in site erection fabrication work
out and you have to a conclusion of your site condition and situation.

Volume of electrodes consumption you can take from electrode
manufacturer.

Muthu Barathi P
Senior Manager QA/QC
AFCONS

On Mon, 27 Sep 2010 13:27:39 +0530 wrote
>Dear All

 

Can anyone advise me on standard productivity norms for
a welder in a vertical tank construction? Please note that the entire
tank is being
constructed using the SMAW process.

 

Best regards    Venugopal Kurup


  +974 33699379





--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

P Muthu Barathi
Mobile No:09967300544

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...