[MW:7200] RE: 7198] effect of longer holding time during hydrotest

ASME B31.3 only require 10 minuttes hydrotest.
That is fully enough for a strength test - and in most cases also for a hydrostatic leak test.
 
But some companies (contractors, costumers) require 30 minuttes test, some 1 hour. It will normally be stated in procedures as part of an ISO 9000 quality system.
 
regards
Kristian


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: 26. september 2010 07:06
To: materials-welding@googlegroups.com
Subject: [MW:7198] effect of longer holding time during hydrotest

Dear All
 
Goodday.
 
 
On what basis holding duration (eg.1 hour, 2hour etc) of hydrotest is decided.
 
 
What will be the effect on mechanical proerty of material if the holding period exceeds than as required by design.
 
eg. suppose for a particular hydrotest  holding period is 2 hours and actual holding period exceeds to 3 hours. what will be the effect on mechanical proerty.
 
 
Thanks in advance for your valuable suggestions.
 
Best Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...