Can any body tell why 20MnMoNi55 material-Quenched and tempered-Forged is most preferable for manufacturing of Steam Generator for nuclear power plant.
 
Note that this is DIN classified material equivalent to P3-SA533 Class 1 of ASME classification.

--
REGARDS,
MAULIK H. THAKKAR
WELDING ENGINEER
LARSEN & TOUBRO
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...