PT is enough; based on the size and thickness we can opt for UT too if
needed.

Thanks
Senthil

On May 19, 7:51 pm, gabsi fathi <gab...@gmail.com> wrote:
> dear ِِAll
>
> As you  know some valve manufacturers use body seat which is welded i.e.
> stainless steel overlay welds over ductile iron body usin MIG welding
> process. the NDT method used to inspect the weld is PT. My question is this
> enough and accepted or you need additional NDT test such as UT.
>  ------------------------------
>  please let me know.
>
> --
> Meilleures Salutations.
> Fathi Gabsi.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...