Skip to main content

[MW:2209] Re: 2198] Full Penetration Weld Test On Assemble Valve

As manufacturer already says it will increase tension and material structure, pwht is advisable. But if its a test and the customer pays, execute and report.

regards,

AJ


Date: Mon, 18 May 2009 14:13:15 +0800
Subject: [MW:2199] Re: 2198] Full Penetration Weld Test On Assemble Valve
From: arlie327@gmail.com
To: materials-welding@googlegroups.com

Customer require Full Penetration Weld on Valve. However, manufacturer response as below..
 
To carry out the FPW on the valve with ASTM A351CF8C is not advisable. This is because during the process the material will expose to the temperature around 900 deg C.
When the material (ASTM A351CF8C)  expose to the temperature above  700 deg C it will transform or out of shape especially on the  parts like valve disc or valve stem,seat, etc.
This valve also required PWHT and the PWHT is carry out prior to assembling and because of welding bonnet , disassembling , machining and polishing cannot be done.
Therefore we wish to inform you again that it is NOT ADVISABLE to do the FPW.
 
But customer still insist on the test. Please advise.
 

Rgds,
alee

 
On Mon, May 18, 2009 at 2:04 PM, Yeleswarapu, Ravi <Ravi.K.Yeleswarapu@c-a-m.com> wrote:
Mr. Lee – Could you post your question more in detail, as I understand the question – RT can be carried out on weld joint of assembled valve to test the weld full penetration.
 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of a lee
Sent: Monday, May 18, 2009 9:57 AM
To: materials-welding@googlegroups.com
Subject: [MW:2198] Full Penetration Weld Test On Assemble Valve

 

Can Full Penetration Weld test on assembled valve ( ASTM A351CF8C ) ?

 

Please advise.

 

Rgds,

alee


~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
This email message is for the sole use of the intended recipient(s) and may contain confidential and privileged information of Cameron and its Operating Divisions. Any unauthorized use or disclosure is prohibited. If you are not the intended recipient, please contact the sender by reply email and delete and destroy all copies of the original message inclusive of any attachments.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~





Heb jij de nieuwe Messenger nog niet?! Download 'm hier
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...