Hi,

Kindly enligthen of what is meant by Eutectic Electrode.


Regs,

R.Ravi



On 5/11/09, PB HEGDE <hegde.pb@isgec.com> wrote:

Hi!

Welding of this type of material (Used in machine tool ) is very critical and require to be welded by Eutectic type electrode. With proper preheating and technique. (Generally it is of Ni base) . You can approach L& T eutectic  or MAGNA (Austrelian  Co) they have the range of electrodes or Tig wire

Regards

 

Hegde p.B.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sandy kumar
Sent: Monday, May 11, 2009 2:35 PM
To: materials-welding@googlegroups.com
Subject: [MW:2140] SMAW consumable for the welding

 

Hi friends

Can anyone please tell me which SMAW consumable I can use to weld following material combination :-

 

1st material:-

C.

Si.

Mn.

S.

P.

0.50%

0.25%

0.70%

0.05%

0.05%

2nd material :-C=0.355,Si=0.6645,Mn=1.7084,P=.0209,S=0.0326,Cr=0.2083,Ni=0.0333, Mo=0.0314,

Cu=0.0226,Al=0.0182,Ti=0.0177,V=0.0935,Nb=0.0103

Please suggest which I can use if it is not suitable.

Best regards

Sandeep Kumar

 




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...