Dear Mr. H. Malekan,

 I think you could use the electrode  OK 73.68

Massimo Gherardi

QAManager - ESAB Saldatura SPA - Italy


Da: sandy <sandy001987@gmail.com>
A: Materials & Welding <materials-welding@googlegroups.com>
Inviato: Giovedì 28 maggio 2009, 14:37:46
Oggetto: [MW:2274] Re: ESAB


Dear Mr, H.Malekan
Please give chemical  composition, strength, CVN of the material

On May 27, 5:10 pm, Hamed Malekan <ham_male...@yahoo.com> wrote:
> Can some body tell me which electrode in Esab brand suitable for welding                 EN10028-4 13MnNi6-3 ? Is that already used anywhere in the world or not ?
>
> H.Malekan


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...