As Body Seat is made with Overlay Welding that means its made for only Corrosion resistance Properties and the layering will be maximum 3-5 mm thk and during this important is their shouldn't be any crack in Layering and I feel PT is sufficient for Valve Layring and if your Thk is increasing then you can think of UT for Bonding and ...all
 
Abhijit

--- On Tue, 5/19/09, gabsi fathi <gabsif@gmail.com> wrote:

From: gabsi fathi <gabsif@gmail.com>
Subject: [MW:2216] NDT for valve body welded
To: materials-welding@googlegroups.com
Date: Tuesday, May 19, 2009, 8:21 PM

dear ِِAll
 
As you  know some valve manufacturers use body seat which is welded i.e. stainless steel overlay welds over ductile iron body usin MIG welding process. the NDT method used to inspect the weld is PT. My question is this enough and accepted or you need additional NDT test such as UT.

please let me know.


--
Meilleures Salutations.
Fathi Gabsi.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...