You have to follow a WPS to qualify a welder. Your WPS with P45 material will not allow you to weld on P1 material. You have to qualify a Procedure with P1 material with F43 consumable. With that procedure  you can qualify the welder.
 
Regards,
Muhammed Ibrahim 

2009/5/27 tamizazagan nagappan <tamizazagann@gmail.com>


I have wps for P45 material incoloy 825 UNS -08825, ASTM SB 462/464 UNS (N08020) NACE with filler metal F43 SFA 5.14  AWS    Er-Ni-Cr-Mo-3...

Is it possible to qualify the welder with A333 Gr 6 base metal  with filler metal F43  SFA 5.14  AWS    Er-Ni-Cr-Mo-3...

    


--
TAMIL
phone: +77023210394

 




--
TAMIL
phone: +77023210394

 Save a tree...please don't print this e-mail unless you really need toRegards







--
Thanks & Regards
Muhammed Ibrahim PK

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...