Yes, The welders can be qualfied using P1 materail unless other essential variables are not Changed.
SB
On Thu, May 28, 2009 at 7:14 AM, Shank Vagal <nach_sam@yahoo.com> wrote:
WQT aims at judging welder's ability to deposit sound weld using a given electrode/filler and the qualified process per the WPS. The material on which to deposit does not matter.
--- On Thu, 28/5/09, Sukamal Naskar <sukamalbecmet@gmail.com> wrote:
From: Sukamal Naskar <sukamalbecmet@gmail.com>
Subject: [MW:2265] Re: about WQT Date: Thursday, 28 May, 2009, 10:44 AM
According to QW-423.1 & QW-433, you can qualify the welder for P No. 1
material using F No.43 consumable. As long as your are not changing
the process GTAW, the welder can be qualified , provided other
essential variables of the GTAW process for the welder qualification
doesn't change.
Regards,
SUKAMAL NASKAR
WELDING ENGINEER
On 5/28/09, Muhammed Ibrahim <ibratech@gmail.com> wrote:
> You have to follow a WPS to qualify a welder.. Your WPS with P45 material
> will not allow you to weld on P1 material. You have to qualify a Procedure
> with P1 material with F43 consumable. With that procedure you can qualify
> the welder.
>
> Regards,
> Muhammed Ibrahim
>
> 2009/5/27 tamizazagan nagappan <tamizazagann@gmail.com>
>
>>
>>
>> I have wps for P45 material incoloy 825 UNS -08825, ASTM SB 462/464 UNS
>> (N08020) NACE with filler metal F43 SFA 5.14 AWS Er-Ni-Cr-Mo-3...
>>
>> Is it possible to qualify the welder with A333 Gr 6 base metal with
>> filler
>> metal F43 SFA 5.14 AWS Er-Ni-Cr-Mo-3...
>>
>>
>>
>> --
>> TAMIL
>> phone: +77023210394
>>
>>
>>
>>
>>
>>
>> --
>> TAMIL
>> phone: +77023210394
>>
>> Save a tree...please don't print this e-mail unless you really need
>> toRegards
>>
>>
>>
>> >
>>
>
>
> --
> Thanks & Regards
> Muhammed Ibrahim PK
>
> >
>
--
Sukamal Naskar
MalaysiaEnter now!
Cricket on your mind? Visit the ultimate cricket website.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments