NO,SEE SEC IX article 2&3 for essential variables for welding procedure and performance qualification. 

From: tamizazagan nagappan <tamizazagann@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 27 May, 2009 6:00:06 PM
Subject: [MW:2250] about WQT



I have wps for P45 material incoloy 825 UNS -08825, ASTM SB 462/464 UNS (N08020) NACE with filler metal F43 SFA 5.14  AWS    Er-Ni-Cr-Mo-3...

Is it possible to qualify the welder with A333 Gr 6 base metal  with filler metal F43  SFA 5.14  AWS    Er-Ni-Cr-Mo-3...

    


--
TAMIL
phone: +77023210394

 




--
TAMIL
phone: +77023210394

 Save a tree...please don't print this e-mail unless you really need toRegards






Cricket on your mind? Visit the ultimate cricket website. Enter now!
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...