CAN ANY BODY EXPLAIN,WHY Y (IN B31.3 FOR CALCULATING THICKNESS) INCREASES WITH INCREASING TEMPRATURE?
(ACCORDING TO ALLOWABLE STRESS DECREASES WITH INCREASING TEMP) 
 