[MW:1444] Re: Cladding Pipe Manufacturer

Sir                                                   Date 10.01.2009
Pl contact sandvik Osprey  UK , They have really High Tech process 7 equpment for doing it
Regards
Suneel Gore

--- On Thu, 8/1/09, rahul.pisat@akersolutions.com <rahul.pisat@akersolutions.com> wrote:
From: rahul.pisat@akersolutions.com <rahul.pisat@akersolutions.com>
Subject: [MW:1436] Cladding Pipe Manufacturer
To: materials-welding@googlegroups.com
Date: Thursday, 8 January, 2009, 3:30 PM

Sirs,
Can anybody guide me for Cladded Pipe manufacturers ? 
I am looking for clad pipe manufacturer with  weld overlay manufacturing process or a Mechanical bonding cladding.
The required material is 30" Pipe with  X70 grade CS and  SS316L grade cladding.
Waiting for information.
Kind reg
Rahul Pisat
Engineer - Material Engineer

This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

Download prohibited? No problem. CHAT from any browser, without download
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...