Skip to main content

[MW:1439] Re: Radiography Test : FULL Vs 100%

Mr.Raghuram is right.UW11 of ASME SEct VIII Div 1 clarifies RT requirements with some exemptions on radiography of Nozzle size upto 8"NB even if the requirement is indicated as "FULL" or "100%".So if R'phy is indiacted as Full or 100% you can always take cognisance of UW11.In literal sense it becomes 100% only when it is specifically indicated that "100% RT for all Butt-welded joints"
Regards
Aarpee
On Thu, Jan 8, 2009 at 4:46 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

No such requirement as 100% in ASME Sec VIII div1, you may refer UW11 for Full RT requirements. Here there are some joints exmpted from RT even you specify as FULL. It depends on designers specific requirements, whether to apply 100% or Full. In my opinion if the datasheet specifies 100% all buttwelds shall be RT'ed irrespective of exmeptions given in UW11(a).


From: Pressure_Vessel@yahoogroups.com [mailto:Pressure_Vessel@yahoogroups.com] On Behalf Of edfarman chan
Sent: Thursday, January 08, 2009 4:45 PM
To: Pressure_Vessel@yahoogroups.com
Subject: [Pressure Vessel] Radiography Test : FULL Vs 100%

 


Dears,

 

Does "Full RT" and "100% RT" has the same meaning of Radiography Test?

If NOT - which section of ASME Sect. VIII Div.1 (or 2 or 3) that describe in detail description for both "Full RT" and "100% RT"? 

Thanks & Regards,
edfarman

__._,_.___





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...