Friday, January 9, 2009

[MW:1439] Re: Radiography Test : FULL Vs 100%

Mr.Raghuram is right.UW11 of ASME SEct VIII Div 1 clarifies RT requirements with some exemptions on radiography of Nozzle size upto 8"NB even if the requirement is indicated as "FULL" or "100%".So if R'phy is indiacted as Full or 100% you can always take cognisance of UW11.In literal sense it becomes 100% only when it is specifically indicated that "100% RT for all Butt-welded joints"
Regards
Aarpee
On Thu, Jan 8, 2009 at 4:46 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

No such requirement as 100% in ASME Sec VIII div1, you may refer UW11 for Full RT requirements. Here there are some joints exmpted from RT even you specify as FULL. It depends on designers specific requirements, whether to apply 100% or Full. In my opinion if the datasheet specifies 100% all buttwelds shall be RT'ed irrespective of exmeptions given in UW11(a).


From: Pressure_Vessel@yahoogroups.com [mailto:Pressure_Vessel@yahoogroups.com] On Behalf Of edfarman chan
Sent: Thursday, January 08, 2009 4:45 PM
To: Pressure_Vessel@yahoogroups.com
Subject: [Pressure Vessel] Radiography Test : FULL Vs 100%

 


Dears,

 

Does "Full RT" and "100% RT" has the same meaning of Radiography Test?

If NOT - which section of ASME Sect. VIII Div.1 (or 2 or 3) that describe in detail description for both "Full RT" and "100% RT"? 

Thanks & Regards,
edfarman

__._,_.___





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...