[MW:1420] Re: ASME B31.3-2006 Ed. Fig. 328.5.2.c

The range is 1.5 - 3mm as per saudi aramco engineering standards.In
B31.3 only approximate gap is given as 1.5mm but no limits specified.
i faced the same problem but w.r.t the max. limit.

Sree
* southern area gas projects *

On 12/24/08, nozhan@cimtas.com.tr <nozhan@cimtas.com.tr> wrote:
>
>
> (Embedded image moved to file: pic14310.jpg)
> After welding, less than 1.5 mm gap is the cause to reject the weld after
> RT?
> If yes, in accordance which criteria?
>
> Thanks...
>
>
>
> Nebi ÖZHAN
>
> e-mail:nozhan@cimtas.com.tr
> >
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...