Wednesday, December 24, 2008

[MW:1419] Re: ASME B31.3-2006 Ed. Fig. 328.5.2.c

1.5 mm gap is set before welding, it is to accomodate shrinkage after
welding. Of course, gap will be less than 1.5 after welding, but it is
not rejected.

What's the meaning after RT?, it is strange to perform RT on the fillet weld.

Regards,

Tex

2008/12/24 <nozhan@cimtas.com.tr>:
>
>
> (Embedded image moved to file: pic14310.jpg)
> After welding, less than 1.5 mm gap is the cause to reject the weld after
> RT?
> If yes, in accordance which criteria?
>
> Thanks...
>
>
>
> Nebi ÖZHAN
>
> e-mail:nozhan@cimtas.com.tr
> >
>

--
Regards,

T. Rizal Hidayat

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...