Saturday, December 6, 2008

[MW:1388] Re: Calibration, Validation of welding machines as per BS 7570 standard.

Dear R.bose,
Refer API 6A for frequency details.
Thanks and Regards,
K.Rajagopal

 
On 12/2/08, Rituraj Bose <boser2006@gmail.com> wrote:

Dear Mr. Muniyandi,

Will you please inform where I can get the details of this frequencies
for calibration?

Regards,
R. Bose

On Dec 1, 12:22 pm, "Muni Andy" <cmkf...@gmail.com> wrote:
> Dear Friends,
> Welding equipments need calibration i e the ammeter and voltmeter is to be
> calibrated.Frequency is once in 3 months.
> validation is required for the welding process and not for welding
> equipments.
> Regrds,
> C.Muniyandi
>
>
>
> On Mon, Dec 1, 2008 at 11:43 AM, <kata...@bilfal.com> wrote:
>
> > Dear friends,
>
> > I am not very clear about the words Calibration, Validation of welding
> > equipments.
>
> > Calibration is defined in some of the literature as all the operations for
> > the purpose of determining the value or errors of a measuring instruments.
> > (Checking the measuring instruments correctness such as A, V meters)
>
> > where as Validation is defined as all the operations for the purpose of
> > demonstrating that an item of Arc welding equipment or welding system
> > complies with the operating specification for that welding equipment or
> > syestem( Checking the correctness of equipment).
>
> > I seen many fabrication  shops  doing calibration not Validation.
>
> > BS 7575-2000  is also having titile  " Code of Practice for Validation of
> > arc welding equipment".
>
> > Can any body  suggest me  wether welding equipment requires  Calibraion or
> > Validation?
>
> > Regards
>
> > P.K- Hide quoted text -
>
> - Show quoted text -
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...