[MW:1288] RE: 1281] Impact testing values

As a general thumbrule, weld metal impacts will be lower than parent metal
values. This is because of the difference in the grain structures.
Regards

Abby Joseph
Bohler Welding Group India


-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of
Sudipto_Banerjee@fwuk.fwc.com
Sent: 10 November 2008 20:07
To: materials-welding@googlegroups.com
Subject: [MW:1281] Impact testing values


Can anyone tell me whether the impact test value will be same for the
parent metal and the weld metal? or it can be different.

Best Regards,
Sudipto Banerjee
Man. no. B 4974
Equipment Engg. Department
Office no. 0044- (0)118 913 2295


=======================================================
Confidentiality Notice

This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no
other person(s) or organisation(s).
(b) May be confidential, legally privileged and protected in law.
Unauthorised use, copying or disclosure of any of it may be unlawful. If you
have received this communication in error, please contact us immediately by
email at Postmaster@fwuk.fwc.com.
=======================================================

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...