[MW:1325] Re: about heating of ss316 pipe

hi
i think the heating the pipe isn't correct .it may occur sensitization.i think the dropping water play a good role ,that it's decrease the cooling rate in base metal,therefore the possibility of carbide cr decreases.


From: pradip kumar gupta <pkgpanki@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, November 17, 2008 9:32:51 PM
Subject: [MW:1322] about heating of ss316 pipe

we were welding a ss316 pipe ,and there were some water drops so we heated it with gas cutting set to evaporate, was this correct or not? if not then why? can any one tell me what will be effect of heating on ss316 pipe.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...