pl. include appropriate subject line when posting a new querry!
is this contractual requirement, Ni>3%?, what is the service involved?
and what is MDMT (i mean minimum not maximum)?
________________________________
From: kataiah@bilfal.com [mailto:kataiah@bilfal.com]
Sent: Wed 05/11/2008 15:58
To:
Subject:
Shell, SA 537 Cl1 (50 mmThk)
Dished end,SA 537 Cl1
SR Nozzle,SA 350 LF2 2inch to 24 inches (Carbon0.3%;Nickle 3.3 to 3.7 %)
VESSEL IS according to ASME SEC VIII-DIV2-EDN 2007
Max design metal metal temp ; -40degree temperature.
Hydro test pressure: 133.5barg
Impacttest for materials: shell/head materials to be impact tested at -60degree centigrade.
Materials for forgings exempeted asper 3.11.2.
Pwht; yes
ASME U2 STAMPED VESSEL
Inform Specification of Electrode to be used.
Regards
P.Kataiah
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments