[MW:1333] RE: 1330] Welding of HIC tested Plates.

You may see NACE TM0284. It shows sampling of spiral / seam welded pipes [see Figure 3] in which samples for testing do have welds. Same may be used to test a coupon welded with the intended WPS.

 

Regards,

Jignesh Patel

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of kataiah@bilfal.com
Sent: Sunday, November 23, 2008 2:40 PM
To: materials-welding@googlegroups.com
Subject: [MW:1330] Welding of HIC tested Plates.

 


Dear Friends,

Many clients are specifying that  the base materials ( SA516 Gr. 70N) shall be HIC tested. For welding such a plates we are using normal E7018-1 electrodes.

Weld need not to pass HIC testing. Guide me on this subject.

P.K</font


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...