Wednesday, November 26, 2008

[MW:1355] RE: 1354] RE: Buried Fittings

It could be poor design, why you need flanges in a buried pipeline?

Most cost effective will be coal tar wrapping


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Fly Yalung
Sent: Tuesday, November 25, 2008 5:44 PM
To: materials-welding @google
Subject: [MW:1354] RE: Buried Fittings

 

Dear Gentlemen,

Good day to everyone. I have one dilema regarding some fittings to be welded to a pipe and will be buried 1.5 meter below grade surface. Is this right thing to done? If correct what is the most cost effective protection that we can do to protect the buried fittings(example- Flanges).

Best regards,

Fly L. Yalung

Material Egineer

M. A. Al-Kawari Est.

K.S.A.

 




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...