Monday, November 10, 2008

[MW:1277] RE: 1271] Pipes ASTM B165 UNS No 4400

Blank
if you refer table X2.1 sizes up to 8" in SMLS are regularly available. for above 8" its quite common to get welded pipe, I don't know, you may check with other vendors if SMLS in 12" is available.
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of Bagesh Kumar
Sent: Thursday, November 06, 2008 4:48 AM
To: materials-welding@googlegroups.com
Subject: [MW:1271] Pipes ASTM B165 UNS No 4400


Dear All,
                 I have got the requirement of subjected material of 12" Size Sch 10S seamless annealed from Licensor side, I sent enquiries to many vendors out of which one has replied in this manner,

Following the enquiry for this project, you are requesting the following item:

- pipe B165 SMLS BE Annealed SCH10S ASTM B165-NO44000 12"

Actually, this product does not exist as seamless due to the thin thickness of the metal.

We requested alternate of: pipe B725 WELDED Annealed SCH10S  12", And request to accept the deviation,

Although I have kept hold on this matter, I would like to get some other quotes and deviation request also before my proceeding. Meanwhile  would like some views to be thrown on that, as I am not been satisfied by the vendor's condition for the said deviation request, As I do not want to change the material just because of its thinness, and aslo it is of licensor's requirement.

Thanks & Regards.

Bagesh

 

 

 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...