hi dear
according to the type of steel,i suggest that you select a optimum h.i until the coarse grain zone retain low & solution carbide decrease.the optimum h.i depends to the type of process(heat intensity)&thickness.


From: darshan gambhava <dgambhava@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, November 11, 2008 7:45:14 PM
Subject: [MW:1296] effect of heat input

Dear friends ,
I want know about the effect of heat input on notch property of LAS.
especially on Cr-Mo-V steel weld.
so plz let me know that any one have information about it or any one have done some experimental work on it,
what is max heat input that can be applied to the LAS(Cr-Mo-V) to get required impact property as per ASME.
thank you

--
Regards,
Darshan Gambhava


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---