[MW:1302] Re: Casting quality levels

As per ASTM E 446 .

Reference radiograph for this is available.

 

Category AGas porosity; severity levels 1 through 5.

Category B—Sand and slag inclusions; severity levels 1 through 5.

Category C—Shrinkage; 4 types:

 

CA—Severity levels 1 through 5.

CB—Severity levels 1 through 5.

 

CC—Severity levels 1 through 5.

 

CD—Severity levels 1 through 5.

Category DCrack; 1 illustration.

 

Category E—Hot tear; 1 illustration.
Category F—Insert; 1 illustration.
 
Regards, Bhaskar Kale

On 11/12/08, rahul.pisat@akersolutions.com <rahul.pisat@akersolutions.com> wrote:
Hello ,
 
Please guide about the definition of the Casting quality level .
Where I can find about the quality of casting as 1, 2 or 3.
 
Also I am not able to understand the Acceptance level ( or class ) specified in ASME 31.3 Table 302.3.3 D.
 
Where can I find this casting level defined ?
 
kind regards
Rahul Pisat
 

This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...