Monday, November 17, 2008

[MW:1319] Fw: [MW:1317] Re: PWHT soaking time


Dear Sir,

As per Table  QW-253  or QW-254  ( Essential, Supplementary Essential, Nonessential Variables table for different processes),  QW-407.2 is applicable when there is impact testing otherwise it is a non-essential variable  (as per my  understanding). QW-407.2 may not applicable
regards

P.K


----- Forwarded by Kataiah/BelleliSA on 17/11/2008 07:10 ص -----
"Emilio Cerato" <ecerato@hotmail.com>
Sent by: materials-welding@googlegroups.com

16/11/2008 09:27 ص
Please respond to materials-welding

       
        To:        <materials-welding@googlegroups.com>
        cc:        
        Subject:        [MW:1317] Re: PWHT soaking time




Dear Friends,

QW-407.2 Said: The procedure qualification test shall be subjected to PWHT
essentially equivalent to that encountered in the fabrication of production
welds, including at least 80% of the agregate times at temperature(s). The PWHT
total time(s) at temperature(s) may be applied in one heating cycle.

Regards.

Emilio J. M. Cerato
Ingeniero Mecánico
Angel Cassanello 480
S3004EAD Santa Fe
Celular (54) 0342 156131383
Telefax (54) 0342 4601834
email: ecerato@hotmail.com
----- Original Message -----
From: <kataiah@bilfal.com>
To: <materials-welding@googlegroups.com>
Sent: Sunday, November 16, 2008 4:33 AM
Subject: [MW:1313] PWHT soaking time


> Dear Friends,
>
> Is a PQR with soaking time of 1 hrs can support a WPS  with soaking time 3
> hrs. (No Impact requirement).
> Is a PQR with soaking time of 10 hrs can support a WPS  with soaking time
> 3 hrs. (No Impact requirement).
> Is a p
>
> Regards
>
> P.K
> >
>



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...