E6010 is best rod for GI trays Sent from my iPhone On 22-Nov-2022, at 1:44 PM, ahmed adil <ahmed.adil5382@gmail.com> wrote: Dear Vishal Oxyacetylene welding or Thermit welding are suitable for your job Best wishes Ahmed Adil Welding engineer On Mon, 21 Nov 2022, 06:48 Vishal Jaiswal, < vis469jaiswal70@gmail.com > wrote: Dear All, Please suggest wihich welding is sutaible for GI flat bar to GI flat bar used in cable tray and also which WPS is use for -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF6t40-BfGWU15koamWdVZ4NsvN_v7mgs69dDW0V6BE%2BUSHqDA%40mail.gmail.com ...
Materials selection, welding, forming, Heat treatment, corrossion, NDT