When Impact test is Applicable, according to ASME Sec.IX, change in AWS classification is an supplementary essential variable and cannot be changed..
Thanks & Regards
J.Gerald Jayakumar
0091-8838619635
On Saturday, 10 October 2026 at 07:36:48 pm IST, Noble <noblejohny94@gmail.com> wrote:
Dear Experts,
If a PQR is qualified using ER70S-2 with impact testing, can we use the same PQR to prepare a WPS using ER70S-6, since both filler metals fall under the same F-Number and A-Number?
Would this be acceptable under ASME Section IX, or would a new PQR be required?
Your expert opinions and code references would be appreciated.
--https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/4acf9c35-fdfd-4ae8-b59d-ed31182946den%40googlegroups.com.
Comments