Skip to main content

Posts

Re: [MW:33757]

E6010 is best rod for GI trays Sent from my iPhone On 22-Nov-2022, at 1:44 PM, ahmed adil <ahmed.adil5382@gmail.com> wrote:  Dear Vishal Oxyacetylene welding or Thermit welding are suitable for your job Best wishes Ahmed Adil Welding engineer  On Mon, 21 Nov 2022, 06:48 Vishal Jaiswal, < vis469jaiswal70@gmail.com > wrote: Dear All,  Please suggest wihich welding is sutaible for GI flat bar to GI flat bar  used in cable tray and also which WPS is use for  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF6t40-BfGWU15koamWdVZ4NsvN_v7mgs69dDW0V6BE%2BUSHqDA%40mail.gmail.com ...

Re: [MW:33756] SS PIPE ASTM 554 TYPE 304

Dear Expert. Thank you for your information,  If we will use 316L filler wire what is the effect for welding? On Mon, Nov 21, 2022 at 9:56 AM Kannayeram Gnanapandithan < kgpandithan@gmail.com > wrote: 308 THANKS & BEST REGARDS, KG.PANDITHAN, BE, IWE,  CSWIP 3.1, ISO 9712 Level 2 in VT, ASNT-Level II in PT,MT,RT & UT, LA ISO 9001-2015, International Welding Engineer.  CONSULTANT-WELDING & QUALITY Mobile no: +919940739349 On Sat, Nov 12, 2022 at 6:38 PM Simhachalam Battini < simhachalam.battini729@gmail.com > wrote: Dear All, Great to hear from you. Which filler is required to weld ss Pipe to Pipe  ASTM A554 Type 304. Thanks, Regards.   Battini Simhachalam QC Inspector – Quality Dept.  ArRiyadh New Mobility - CWG 6 th Floor, ArRiyadh New Mobility Building Olaya Street (North) – Al Sahafah District P.O. Box 99816 – Riyadh 11625 – Saudi Arabia M +966 546044327 simhachalam.battini@cwg-metro.com www.anm-metro.com 24°46...

[MW:33743] material...@googlegroups.com

Gents H as any body an idea about replacement for fitting after second repair (kindly mention the reference in ASME B31.3?) Rgerdas Mostafa  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0c971df0-ae21-4982-a6e7-2cc8537cef7en%40googlegroups.com .

Re: [MW:33754]

Dear Vishal Oxyacetylene welding or Thermit welding are suitable for your job Best wishes Ahmed Adil Welding engineer  On Mon, 21 Nov 2022, 06:48 Vishal Jaiswal, < vis469jaiswal70@gmail.com > wrote: Dear All,  Please suggest wihich welding is sutaible for GI flat bar to GI flat bar  used in cable tray and also which WPS is use for  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF6t40-BfGWU15koamWdVZ4NsvN_v7mgs69dDW0V6BE%2BUSHqDA%40mail.gmail.com . -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because y...

Re: [MW:33748] material...@googlegroups.com

Greetings, As I know there is no direct reference in ASME B31.3. You can refer to client specifications.  Muhammad Babur Khan Sent from my iPhone On 22 Nov 2022, at 6:28 AM, mostafa...@gmail.com <mostafakamelbp@gmail.com> wrote: Gents H as any body an idea about replacement for fitting after second repair (kindly mention the reference in ASME B31.3?) Rgerdas Mostafa  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0c971df0-ae21-4982-a6e7-2cc8537cef7en%40googlegroups.com .

[MW:33747] Columnar microstructure

Dear expert, Good day.  We did inconel welding, the report states "columnar microstructure were found in weld metal". Can anyone guide me what does that microstructure means?  Enclosed screen shot of the report. Best regards, Pravin  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7dYsF_m_Y-K4dd1cpd92j9qvXW1Q5tr1UXT6GTfqeXwVw%40mail.gmail.com .

Re: [MW:33743] Query on SMAW electrode selection for API 5L X65

use 8010, On Mon, Nov 21, 2022, 4:46 PM Muhammad Azeem < azeem7999@gmail.com > wrote: You can used 7010 root and filling capping 8010.. On Mon, 21 Nov 2022, 13:05 karu...@gmail.com , < karunaqc@gmail.com > wrote: Dear all,         Please suggest API5L X70 GRDE pipeline .Which electrode E7010 or E8010 -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8725c287-0d1d-451b-ae7e-551e5bede9f5n%40googlegroups.com . -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups ...