sour service:nace as per asme b 31.3 pwht not reqd, but in addition to 31.3 also refer NACE MR0103. A106GrB is classified as P no.1. Read para 2.1.8.3 in NACE MR0103 which refers to standard that should be followed for method to prevent excessive weldment hardness. shyam On 2/26/08, Zameer Mohammed < dreamthinkwork@gmail.com > wrote: Dear Mr. Kumar, Thanks for your comments. As per the Piping Spec Pressure BARG : 91 15 Temperature DEG. C: 93 245 Thank you, Regards, Sabir On 2/26/08, Kumar Bagesh (Mumbai - Piping) < B.Kumar@ticb.com > wrote: As per general requirement for PWHT is the Wall thk of Pipe i.e. for CS it should be >= 19 MM, But for your case it looks like Sour Service, In ...
Materials selection, welding, forming, Heat treatment, corrossion, NDT