Re: [MW:35964] WPS requalification for repair weld ASME B31.3

If new PQR qualification as per client specification is there means no need to ask this question, normal & repair PQR should be qualified separately. If we are talking on the basis of ASME SEC 9 & ASME B31. 3, below Explanation is sufficient.


The qualification range would be 16 to 36mm if you qualify a PQR On 18mm plate thickness, PWHT soaking on pqr is 1hr 30mins so maximum soaking with impact will be 1hr 52.5mins, if you are doing the resoaking and if the total soaking time ( Actual PWHT & Repair PWHT soaking time) is within this range you can use this, if it exceeded need to requalify.

The above explanation is based on With impact testing & PWHT below the Lower transformation temperature (AC3)

On Wed, 28 Jan 2026, 6:49 am ananth karuppanan, <ananthkaruppanan91@gmail.com> wrote:
Dear 

New PQR need to be qualified for the repair welding as per the client requirements.

Thanks & Regards,
Ananth Karuppanan.
Mobile : +91-9597936444
               +971-588925593


On Wed, 28 Jan 2026 at 7:49 AM, Babur Khan <mbabur.bwp@gmail.com> wrote:
Greetings,
Need expert opinion for the following query:
Construction Code ASME B31.3, Qualification ASME BPV Sec. IX.
One of the WPS is qualified for Low temperature Carbon steel with impact testing and PWHT. The qualification range is 20mm to 36mm. 
PWHT is applicable (Project specification). Soaking time was 1 hr 30 minutes.
Question: Is this WPS qualified for a repair weld with this soaking time? 
Is a new PQR to qualify the repair joint?

Best Regards,

Muhammad Babur Khan Lashari
Project Quality Supervisor.
API 570, API 510, CSWIP 3.2.2. ISO 9001:2015

Mob: +966 58 2774568 / +966 51 0559680

Please consider the environment before printing this e-mail

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAN53wK16%2Bvf43xPRxmXync%3DGa42jqR7kk70ou7vyCdT9MShcZQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAMK7HtARNaK7E1cR6iZX4FAoep7Eskx_u8G1%3DO9Wx4kCp9zOKQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ90KGRiTXaz78a6CVup7fzWACoLNmV5OMX6iwXT_OSzoXfW1A%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...