Re: [MW:35537] RANGE ASME SEC IX

What is the diameter of the pipe to be welded , ASME IX give a limit on the diameter to be welded by a welder that has been qualified in a plate and what positions they can weld 

On Wed, 16 Apr 2025 at 08:57, Elavarasan Mech <elavarasan1861994@gmail.com> wrote:
Dear All

we have qualified WPS for ( ASME SEC IX)
1. BASE plate 8 mm ( 8TO 16 mm RANGE WITH IMPACT ) 
2 . BASE plate 25 mm ( 16TO 50mm RANGE WITH IMPACT ) 

Qualified WQT BASE PLATE THICKNESS :25 mm 
( 50 mm max ) 
My question is   Can we use this plate WPS and WQT  to weld 24inch pipe (9.5mm wall thickness )and 26 pipe(14mm wall thickness ) ,Welder can weld 8 mm wall thickness pipe ?                                  he qualified in 25 mm plate only  .please quide me

Regard 
ELAVARASAN


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ymSZ4aGa3XqiJswKMyr0sqCGWJO6xfGf_NCpqTSNFN5-A%40mail.gmail.com.


--
Thanks & kind regards


EmailLogo      

www.ahkgroup.com     

    
     Rilley Chellah Mulenga
     HEAD - MATERIALS EVALUATION

     T: +260 212 226431
     M:+26076123880/ 0964084833
     E:Rilley.Mulenga@ahkgroup.com


DISCLAIMER: The information in this Internet e-mail is confidential and may be legally privileged. It is intended solely for the addressee(s).
Access to this Internet e-mail by anyone else is unauthorised.

If you are not the intended recipient, any disclosure, copying, distribution or any action taken or omitted to be taken in reliance on it, is prohibited and may be unlawful.
All results and data contained in this document are subject to our Standard Terms and Conditions and are valid only when supported by an original document.

Please visit our website at www.ahkgroup.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHkXHT_qMzt7TESHXC2-%3DM3_7gmsbCznt5h4MhkxwYu7-GzNtg%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...