Re: [MW:35517] Welder Qualification as per ASME SEC IX E6010-E7018

Two times of the deposit material thickness.

On Sun, 6 Apr 2025, 6:49 pm ROLANDO RC, <soldadurasrc@gmail.com> wrote:
Good morning, group. I'm asking for your help with the following topic: ASME IX Welder qualification:
- 3" Sch 80 pipe - SMAW E6010 (t: 2.62 mm) - SMAW E7018 (t: 5 mm) What is the qualification range for F3 and F4?
Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1d3d6208-ab11-4466-8074-b06af7932050n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKkuHjuJ3W6yPykmxoo9pWkSm%2BwskMTO7%3DDHLrPBMNN1uw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...