Wednesday, April 2, 2025

[MW:35502] SAW WELDING


Dear Expert 


what are the minimum thickness can qualify SAW welding .8mm thick plate  possible to weld  ( GTAW -4mm & SAW 4 mm ) 
We choose F7A5-EM12k combination please guide me 

Regards 
Elavarasan

--