Dear Experts,

I am following up on my earlier emails regarding the alignment of weld seams on SS304 pipes and their reinforcing pads (RF pad). I have not yet received a response and would greatly appreciate your expert opinion on the matter.

To recap: Is aligning the EFW seam of the pipe with the manually welded seam of the RF pad in the same straight line acceptable per ASME standards?

Are there any minimum distance requirements between the pipe seam and the RF pad weld joint, as per the relevant ASME code sections?

Your prompt guidance would be greatly appreciated to ensure compliance with the necessary standards.

Thank you again for your time, and I look forward to your response.


Best regards,
Vinoth G


On Thu, 27 Mar 2025 at 20:23, Vinoth Kanna <gvinoth43@gmail.com> wrote:
Dear Experts,

I would like to seek clarification regarding the alignment of the weld seams on SS304 pipes and their reinforcing pads (RF pad). Referring to the attached photo, the EFW seam of the pipe and the manually welded seam of the RF pad are aligned in the same straight line.

Could you please confirm whether this is acceptable as per ASME standards? Also I would appreciate it if you could specify the relevant ASME code section and highlight if there is any minimum distance requirement between the pipe seam and the RF pad weld joint.

Your expert guidance on this matter will be highly valuable.


Best regards,

Vinoth G

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BoUWirva1vFd87uHFquQO%2BO_2wSubqTWyg2q2hcwoXTu-sNTQ%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...