Yes, Correct.
Manoj
On Mon, 7 Apr 2025, 14:58 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Thanks for the your replywe have qualified WPS for 8 mm & 25 mm plate with impact (8-16 mm range & 16-50 mm ) as per ASME sec IX now I'm qualifie my welder 25 mm plate ( 5-50 mm range ) with and without impact doesn't matter my interpretations is correctRegardsELAVARASAN--On Mon, 7 Apr 2025 at 1:14 PM Deerendra Karanth <dkaranths@gmail.com> wrote:QW-303.1 clearly states that "Welder performance qualification test need not include impact testing, even if the WPS requires it
Welder can be qualified without impact testing, as long as he welds a test coupon per the WPS.
But, you must ensure that the welder uses an impact-tested WPS when making production welds that require impact properties.
BR
Deerendra
--On Mon, 7 Apr, 2025, 13:32 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:Dear Expertwe have qualified WPS for 8 mm & 25 mm plate with impact (8-16 mm range & 16-50 mm ) as per ASME sec IXWhat about the welder qualifications we need to be consider impact requirement same as per WPS or impact requirements doesn't required for welder qualifications please guide meRegardsELAVARASAN--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4yma_rkksaAF0azyoL7jbiNNjZrp3taCiuHHWdumPT5mMg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9E%2BEeXH5EWeWcEmESFevgN%3D%3D%2B9t31D%3Deg5c-eA9wgudTQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ykS5iBLZg6_6SanWjEZL2ugAgxdV4Hh6iGM_-SAXS2A0g%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACgUO5kx55dtKSS6i_oR_ANmVF__bWindQJ3mF9YMQVFdqdC-Q%40mail.gmail.com.
Comments