Re: [MW:35520] Need Advice – Zirconium Overlay (ERZr-2) on 316L SS Using GTAW

we do welding ( shrink fittings) of Zicronium tube to SS316.

On Mon, 7 Apr 2025, 09:58 Amit Udavant, <amitudavant@gmail.com> wrote:
Shrink fit of what?

Shrink fit of shafts is a regular practice 
Amit

On Mon, 7 Apr 2025, 09:47 patni engineers, <patniengineers@gmail.com> wrote:

Shrink fitting possible ?


On Sun, 6 Apr 2025, 23:39 Hamid Firoozi, <firoozihamid6@gmail.com> wrote:
I'm working on a project involving ERZr-2 overlay on 316L stainless steel using the GTAW process. As many of you know, zirconium is highly reactive—metallic contamination and overheating can easily cause cracks or oxidation that affect weld quality. We've tried ERNi-1 (nickel) as a buffer layer, but experienced crystallized cracking and gummy melting, leading to lack of fusion. .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/f9b005d9-932d-450f-86f5-aa6d82bae758n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKLNAG4LjtU3NL%2Buw_de_nM2T8S6OUBbXvCMuxqFxuqk6U9kCA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAABv9LB%3DuCvJVmiKtBX1ezN_jciR%2BuSLYtR75SpPXfPunb%3DJUw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKLNAG5obo7PwDH_7AVuRMrLyY__iFXs3gKGDCNsv-jUi6SR0Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...