Skip to main content

Re: [MW:35505] Re: Clarification on SS304 Pipe EFW and RF Pad Weld Alignment per ASME Standards

Dear Mr. Vinoth,
Aligning the Extruded Finned Weld (EFW) seam of a pipe with manually welded seam of RF pad in the 
same straight line is generally not recommended as per ASME standards. 
ASME B31.3 and ASME Sec. VIII do not explicitly prohibit it, they emphasize avoiding stress concentration 
points that could lead to failure.
Playing both seams in alignment may create a weak point, increasing a likelihood of crack initiation or failure 
under stress, cyclic loading or thermal expansion.  
Closely aligned seams can make NDE more challenging and may miss incomplete fusion or other defects.
ASME B31.3 (sec. 328.5.4) recommends seams should be staggered to avoid stress risers.
A good engineering practice is to maintain  a 50 mm staggering of the seams based on service conditions and 
material. 
Hence,
1. Off set the seams to minimise the stress concentration.
2. Perform RT, UT, PT to verify the weld integrity if alignment (maintaining the minimum distance) is not possible.
3. Industrial standard recommends a min. of 50 mm or 1.5 to 2 times  the thickness of pipe seam and the RF 
    pad weld for separation to reduce stress concentration. 
4. Otherwise follow client requirements for exact values.
Trust it is clear.
rgds,
C Sridhar.
---------------------------------------------------------------------------------------------------------------------------------------
      



On Thu, 3 Apr 2025 at 09:46, Vinoth Kanna <gvinoth43@gmail.com> wrote:

Dear Experts,

I am following up on my earlier emails regarding the alignment of weld seams on SS304 pipes and their reinforcing pads (RF pad). I have not yet received a response and would greatly appreciate your expert opinion on the matter.

To recap: Is aligning the EFW seam of the pipe with the manually welded seam of the RF pad in the same straight line acceptable per ASME standards?

Are there any minimum distance requirements between the pipe seam and the RF pad weld joint, as per the relevant ASME code sections?

Your prompt guidance would be greatly appreciated to ensure compliance with the necessary standards.

Thank you again for your time, and I look forward to your response.


Best regards,
Vinoth G


On Thu, 27 Mar 2025 at 20:23, Vinoth Kanna <gvinoth43@gmail.com> wrote:
Dear Experts,

I would like to seek clarification regarding the alignment of the weld seams on SS304 pipes and their reinforcing pads (RF pad). Referring to the attached photo, the EFW seam of the pipe and the manually welded seam of the RF pad are aligned in the same straight line.

Could you please confirm whether this is acceptable as per ASME standards? Also I would appreciate it if you could specify the relevant ASME code section and highlight if there is any minimum distance requirement between the pipe seam and the RF pad weld joint.

Your expert guidance on this matter will be highly valuable.


Best regards,

Vinoth G

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BoUWirva1vFd87uHFquQO%2BO_2wSubqTWyg2q2hcwoXTu-sNTQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYigy2N23KgwxiT6qK694zUOMg9zYv21wKiGNEsCJrLHkBA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...