Re: [MW:35048] Difference of 2% of Chromium Content on the Actual PMI VS Sec IIA

It's is acceptable 

On Fri, 31 May 2024, 10:11 pradip kumar Sil, <pradipsil@gmail.com> wrote:
You can refer PFI  ( Pipe fabrication Institute ) or 10 % bi lateral tolerance of actual alloy content from code for the base metal.

On Fri, May 17, 2024 at 12:14 PM Dinesh Baskaran <dinesh09nov@gmail.com> wrote:

Plz refer attach 

Thank and regards

Dinesh Baskaran


On Thu, 16 May, 2024, 12:05 pm Macario Jr. Palola, <macario.palola@gmec.ph> wrote:
Sirs,

May I ask your valuable inputs with regards to my queries.
Base on the attached report, the actual value of %Cr is 20% as per PMI and the value of %Cr in ASME Sec IIA. Now my question, is this acceptable or not ?

Thank you in advance.

Regards,

Mac

The information contained in this email is intended for use only by the recipient to whom or which this is addressed. Such information may be privileged, confidential, and/or proprietary subject to the GMEC Email Disclaimer. Moreover, as we value your privacy, we will handle and safeguard any personal data we receive in this email in accordance with our Privacy Notice.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a98f67f1-0f70-4e02-ac62-785bd8abddf1n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMAJDVoHNBxpdntmSf%2B%3DYPP0LZ4sEZLUsw6dY_46eDr4xdU43w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8nXoiE-wYcMf_9Cj9MArocd11vsmdLy-MwSK3CoMON5yQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGr8UaZ-GJnYGbrQjozc1kHTyutwTvuOJSUxCuqzKLmHGaO%3DrQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .