Saturday, December 9, 2023

Re: [MW:34696] Increase in soaking time

The question is generic.
To answer the query , you may refer below 
For production weld PWHT, construction codes like  ASME SEC I PW 39 . ASME sec VIII DIV 1 UCS 56 are referred.
The holding time at the specified temperature range is followed  as a Minimum from respective Tables in the Codes  .
15 - 20 minutes more than minimum specified is acceptable and no issue is envisaged 
Vishwas Keskar 
IWE 

Sent from my iPhone

On 08-Dec-2023, at 11:24 PM, kumar sumit <kumarsumities@gmail.com> wrote:


Dear sir
              In Pwht if soaking time period is increase(I.e- 15-20minute) at that time it is accepted or not. If accepted then how. If not accepted then also explain. Because I also search in sec IX but I cannot find.
                      Please explain. 
I thankful to you. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACCHnjW3O9wLgzTBzRFZr78FLdCqgafkhxUKjyd3GSBQPsnZiQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...