Yes, we can do that, as per guidelines of IS 2062 we have to retest 2 different sample selected from 2 random location,
But these 2 sample must be pass the specifications.

Reference given in IS 2062 itself.

On Wed, 6 Dec, 2023, 9:34 am Rahul Chaudhari, <chaudharire@gmail.com> wrote:
Dear expert, I have one concern... IS 2062 plate has rejected in tensile test at Lab. So can we retest the same plate again for revaluation? iF yes, where it has been mentioned in code?? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/KL1PR02MB7286D3B36750FBE47E6B4263A485A%40KL1PR02MB7286.apcprd02.prod.outlook.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADmp_wOva_BZ3%2B%3Dt%2BZQCqK8RDcTOrb0ALdzPXG9gSy8g%2Bf5_RA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...